In situ tensile and creep testing of lithiated silicon nanowires (vol 103, 263906, 2013)

TitleIn situ tensile and creep testing of lithiated silicon nanowires (vol 103, 263906, 2013)
Publication TypeJournal Article
Year of Publication2014
AuthorsBoles, ST, Thompson, CV, Kraft, O, Moenig, R
JournalApplied Physics Letters
Volume104
Issue9
Date Published2014/03/03/
ISBN Number0003-6951