THE POTENTIAL FOR CMCS TO REPLACE SUPERALLOYS IN ENGINE EXHAUST DUCTS

TitleTHE POTENTIAL FOR CMCS TO REPLACE SUPERALLOYS IN ENGINE EXHAUST DUCTS
Publication TypeJournal Article
Year of Publication1994
AuthorsRoth, R, Clark, JP, FIELD, FR
JournalJom-Journal of the Minerals Metals & Materials Society
Volume46
Issue1
Pagination32 - 34
Date Published1994/01//
ISBN Number1047-4838